fig3

Reconstruction-mediated interfacial water engineering in Cu-Mo electrocatalyst for highly efficient and durable water splitting

Figure 3. Electrochemical performance of HER and OER. (A) LSV curves; (B) Overpotentials; (C) Tafel plots; (D) EIS spectra; (E) Cdl values of Cu-MoS2 and control catalysts for HER; (F) Chronopotentiometric curve of Cu-MoS2 at 500 mA cm-2 for 100 h; (G) LSV curves; (H) Overpotentials; (I) Tafel plots; (J) EIS spectra; (K) Cdl values of CuO-MoS2/MoO3 and control catalysts for OER; (L) Chronopotentiometric curve of CuO-MoS2/MoO3 at 500 mA cm-2 for 100 h.